ASTM International | BSi - British Standards institute | Material |
A120 | 1387 (BS EN 10255:2004) | Carbon Steel |
A53 Gr. A | 3601/320 | Carbon Steel |
A53 Gr. B | 3601/410 | Carbon Steel |
A106 Gr. A | 3602/360 | Carbon Steel |
A106 Gr. B | 3602/410 | Carbon Steel |
A333 Gr. 3 | 3603/503 | Killed Carbon Steel |
A333 Gr. 6 | 3603/410 | |
A333 Gr. 8 | 3603/590 | 3.5% nickel |
API 5L Gr. A | 3601/23 | Carbon Steel |
API 5L Gr. B | 3601/27 | Carbon Steel |
A335 Gr. P5 | 3604/625 | 5% Cr 1/2% Mo |
A335 Br. P9 | 3604/629 | 9% Cr 1% Mo |
A335 Gr. P11 | 3604/621 | 1 1/4% Cr 1/2% Mo |
A335 Gr. P12 | 3604/620 | 1% Cr 1/2% Mo |
A335 Gr. P22 | 3604/622 | 2 1/4% Cr 1% No |
A312 Gr. Tp 304 | 3605/304 S18 (EN58E) | Austenitic chromium nickel |
A312 Gr. Tp 304H | 3605/304 S59 | Austenitic chromium nickel |
A312 Gr. Tp 304L | 3605/304 S14 | Austenitic chromium nickel (extra low carbon) |
A312 Gr. Tp 316 | 3605/316 S18 (EN58J) | Austenitic chromium nickel molybdenum bearing |
A312 Gr.Tp 316L | 3605/316 S14 | Austenitic chromium nickel molybdenum bearing (extra low carbon) |
A312 Gr. Tp 321 | 3605/321 S18 (EN58B) | Austenitic chromium nickel titanium stabilized |
A312 Gr. Tp 347 | 3605/347 S18 (EN58G) | Austenitic chromium nickel nobelium stabilized |